Sharprite Wire Resharpening Device
 

Trial Study

Make of Card

Mixing

Throughput Before
Resharpening
After
Resharpening
Improvement
Rieter C4 Akala
40's
280T
430T
N.R.E. - 86.6%
N.R.E. - 85.1%
N.R.E. - 91.1%
N.R.E. - 88.6%
N.R.E Improved by 3.5% - 4.5%
 
Crosrol MKV NHH 44 /
AHH
30'sKH
380T

U%       : 13.18
Thin       : 23
Thick     : 233
Nep       : 438

13.12
20
229
375
Total Imperfections Improved by 22.4%

Total      : 805

624
 
LC 300A 100's
Combed
310T

U%       : 15.6
Thin       : 95
Thick     : 283
Nep       : 319

14.8
82
225
211

Total Imperfections Improved by 25.6%

Total      : 696

518
 
Trumac DK 780 56's
Combed
260T

U%       : 16.26
Thin       : 2
Thick     : 41
Nep       : 117

16.23
1
36
101
Total Imperfections Improved by 13.7%

Total      : 160

138
 
L.R.C1/3 38's
Carded
320T

U%       : 15.98
Thin       : 126
Thick     : 705
Nep       : 820

15.36
100
629
696
Total Imperfections Improved by 12.3%

Total      : 1651

1425
 
Trutzsch.DK740 30's Grey
Melange
 

U%       : 14.82
Thin       : 26
Thick     : 178
Nep       : 382

14.23
19
121
229
Total Imperfections Improved by 37%

Total      : 586

369
 
LC 100 30's Carded 150T

Neps/gm : 93

Neps/gm : 72

Improved
 
Trumac DK780 40's KHY 800T

U%       : 14.09
Thin       : 77
Thick     : 525
Nep       : 988

13.91
50
501
893
Total Imperfections Improved by 9.1%

Total      : 1590

1444